Take a account of ARC Efficiency in calculating heat input
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Jun 21, 2016 at 5:19 PM, George Dilintas <dilintas@gmail.com> wrote:
GTAW pulsed--2016-06-20 12:23 GMT+03:00 Kalimuthu Selvaraj <kalimuthube@gmail.com>:--Experts,Kindly order the below welding processes from lowest heat input to Highest heat input.GTAW Pulse, GTAW, SMAW, GMAW short circuit, GMAW pulse.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bcebd94c-8d61-4fc8-8d6f-3b1fe49c61f0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--Dr. Georgios Dilintas,Dipl. Ing. In Aeronautic and Space EngineeringPh.D in Mechanics of Solids - Computational MechanicsA.I.S, A.N.I, IRCA Lead AuditorWelding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40A3MphYNidds_h-h-zwtAoKSoJHK8AdRH3M6j%2BjT_y1%3DQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNwR-mZ4H%3De58aRKkSj9GcSQ69tW_3i1-rQ3f45La32ug%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments