[MW:25002] Welder Qualification (ASME Sec.IX welder can use API 1104 WPS)

Dear All,

We want to know about Welder qualification construction code is  B31.8 whereas WPS as per API 1104 and welder qualified as per ASME Sec. IX.
Project Well Heads and Facility work
Construction Code ASME B31.1 & B31.8
As per B31.8 for repair weld WPS shall be on API 1104.

Now We Have PQR material Client provided 16"x Sch.STD (9.53mm)
For 16'' Dia. Min 2 welders weld a joint.
These two welders qualify on all positions? (Ref. required because in API 1104 we not found).
2nd option is we use API 1104 WPS and Welder ASME Sec. IX qualified we can use?
Waiting for Your prompt response.  

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector

(CSWIP 3.1 / CWI II From PWI) 

 Khaled Juffli Industial Company

Mob: + 966 56 2179280 / 58 2774568

PAK : + 92 334 6186285

Skype: babur.lashari

E-Mail: babur.khan@kjgroup.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN53wK1SLXQJzxVZpuCk_yJLMq_Pq0Gsopjn%3DVHFUcQsYRMHoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...