PQR on P1Gr1 to P1Gr2 qualifies welding P1Gr1 to P1Gr2 only and NOT welding to themselves i.e ( P1Gr.1 To P1Gr1 Or P1Gr2 to P1Gr2)
Refer ASME interpretation IX-92-70 on the same subject.I could not find downlodable copy.Try to search on internet.
Thanks
Mohammed
On Friday, 17 June 2016 1:52 PM, "nithindsilva4u@gmail.com" <nithindsilva4u@gmail.com> wrote:
P1 G1 to P1 G2 qualifies P1 G1 to P1 G2, P1 G2 to P1 G2 and P1 G1 to P1 G1. Hope your query is addressed.
Sent from my iPhone
--also please advice i need to qualify group 1 separate and group 2 separate PQR.or only this PQR is qualified group 1 to group-2 qualified.based on above i need your experience If iam qualified PQR p1 group-1 to p1 group-2 tow different group welded it self so the qualfied range will be p1 group1 and p1 group 2.Dear All,As per ASME SEC-IX change in material Group is Supplementry essential variable (403.5)
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1csg3Drkobg2%3DG9Lyy0CMd3WbM%2BOq_9e2GkJLoC-QxBUhP0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0232776F-14AF-4FF0-8B7E-DA998585BF07%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0232776F-14AF-4FF0-8B7E-DA998585BF07%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments