Tuesday, June 21, 2016

Re: [MW:24984] P8 material WPS to comply QW 407.2_PWHT temperature_time

You have to read QW-407.1. 
according to this paragraph for P-number 8 it is up to you to define the "specified temperature range". So, remember that ASME BPVC is not a Handbook and look in the bibliography what is the acceptable temperature range for solution annealing

2016-06-19 20:59 GMT+03:00 Praveen Kumar <praveenkumar.tkm@gmail.com>:
Dear Mani

If you have impact requirements the clause 407,2 also applies , in that case  the requirement of new pqr is needed. 
Secondly the long soaking time of 7 hours , will have some deteriorating effect on ASS, Kindly check that also. 

On Saturday, June 4, 2016 at 10:06:18 AM UTC+4, jaya anil wrote:
In this case , you need to qualify new PQR. 

Read ASME Section IX QW 407..clauses.

On Sat, Jun 4, 2016 at 5:49 AM, manivannan hemu <hemuman...@gmail.com> wrote:



Dear All,


I have a Query.


We have a SMAW-WPS [ASME SEC IX] for material P8/G1 – PQR with CHARPY tested. In this PQR it was post weld heat treated to re solution anneal at 1090 DEG C for 2 Hrs.


Now we have new production weld requirement  on a part of 8 inch thick with PWHT [solution anneal] at temperature 1130 DEG C and soak time of 7 hrs.


Please clarify me, is it acceptable to revise the WPS [with the same PQR] to address PWHT temperature as 1130 DEG C, and time as 7 hrs to utilize for the new production weld.


In doing this I considered QW407.1(b) (2) 'PWHT within specified temperature range' – in this case specified temperature range for solution anneal as 1040 DEG C minimum by ASTM A351, and NO maximum is specified.


I appreciate your response with the intent requirement of QW 407.2


Regards, MANIVANNAN.P

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5432c488-6730-400a-8abc-0ef4a78db4d3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f882c533-7856-479d-921f-be4c9695c0f3%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CxeYmGfmSW3-jEVSd9b5jW2jFj-Gt1Bgd%2BXSWGRmrXtA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...