Thursday, June 16, 2016

[MW:24963] Pressure vessel (Sphere) shell weld joint 2nd time repair observed after attained 1st repair works

Dear Sir/Expert,

We doing spherical tank (Sphere) constructions at our current projects at India, our constructions code ASME Section -  Vİİİ Div-2,
Materials thickness 45mm, As per constructions requirements materials shall be simulated PWHT(3-Cycle pwht),
Design temp -34deg. C

My queries,
1. Why simulations PWHT(3-cycle) materials is required for constructions
2. Before PWHT how many times repair will be permits. 
3. After PHWT how many times repair will be permits
4. After PWHT if repair will be observed on that times after attain the repair works what is the requirements of PWHT.

Requested all of you please reply with code reference 

--
Thanks & Regards
Pinaki Boxi.
*Mob :- +905351054384.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TAGmF6Uq73Lrq9t__vuXg0A%3DbXyytPzMLOpQLs5FyeirQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...