Here we are the client. There should be some regulatory requirements?Thanks for all your contribution.  
Regards, S.SENTHILKUMAR


On Wednesday, 15 June 2016 8:41 AM, Perumal Govindan <perumalgovindan@gmail.com> wrote:


Dear Senthil
Only solution is discuss with the Client and close if the repair is not connected or in contact with the process medium flow (wet part).
On the otherhand please go through NBR instructions.
Regards
Govindan
On 15 Jun 2016 07:27, "'SENTHILKUMAR SWAMINATHAN' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
We have an issue in repair a pressure vessel.
Contractor not capable to do? But contractor is qualified for R-Stamp.
As company can we  go head in welding activities with our qualified welders and we don't want R Stamp - Is it acceptable? Because this activities ongoing in offshore shut down and we cannot wait as per schedule. I day barge cost is 3 million USD

Thanks
Regards,
S.SENTHILKUMAR
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1914300373.2435806.1465964614944.JavaMail.yahoo%40mail.yahoo.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9eXkjRqVmJZy0aRJ5aTjsuRKH9aLVQg1eYQY_uMSnzABg%40mail.gmail.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...