A new WPS is to made (say WPS-B) for GTAW.

When you are welding a joint where only GTAW is to be used then you have to use WPS-B and when you have to weld GTAW + SMAW then WPS-A to be followed.

Separate WPS are to be maintained because of this reasons. No code references for this.

When you are welding only with GTAW and mentioning WPS-A will make a misunderstanding that it is welded with GTAW + SMAW.

So my opinion is to make a new WPS with the same PQR and maintain both WPS depends on the process you are using to weld.

Regards,

Hareesh K V
+91-8547859202

On 29 Jun 2016 9:10 am, "Rajesh S.Mhaske,Engineer Welding,CSWIP,ASNT,Pune," <rajesh.mhaske17@gmail.com> wrote:
Dear
  Not required to prepared the New WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fc45dd8b-3141-4740-859f-7fa308a4923a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAUbkZdnHYfRWhOtQcLJhic%3DU-H%3DFVZGcCHTHOpUs5X%2BbA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...