what is your qulaified PQR weld sequence? i guess weld the P1 material first and clad restoration on top it
do u need new WPS for clad restoration or groove weld? any way either case you need to qualify new PQR
On Tue, Jun 14, 2016 at 5:33 AM, Hareesh K V <hareesh13h@gmail.com> wrote:Dear all,we have qualified a PQR (groove weld) for clad material (SA 240 410S (Clad) to Carbon Steel that is P7 to P1 material) using ER 309L Mo for the clad portion and E7018 for the rest.Now we have to weld SA240 410S to SA240 410 S material for another job.My question is, can we use the above said qualified PQR to make a wps of SA240 410S to SA240 410 S material, as other variables are same.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkZZU%2Bw8VVA1vAMT1PWD0BDBavujb4OOxwfivKOW2WUYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments