yes, A major change in joint design constitutes an essential variable. (although it's  vague definition in API 1104, it considers all set in/set on etc. are fillet welds) 

On Wednesday, 15 June 2016 15:18:04 UTC+4, waqas suleman wrote:
Dear Members,

We qualify our WPS on Single V Butt joint design, my concern is that can we use this WPS for fillet welding too.
As per API 1104 SECTION 5.7, 5.8 describing about Fillet weld welding requirement.

Regards,

Waqas Suleman

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e9095194-0a65-46c1-84ca-0828cdf73668%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...