[MW:24998] RE: RE : Re: Fracture test

Hi,

For acceptance criteria please refer QW-182.

 
 


Thank you.

Regards,
Dhanasekaran S,

Aker Solutions.

Mob: +91 75079 17709  I   +91 70401 02428 






Date: Wed, 22 Jun 2016 22:58:47 +0100
Subject: RE : Re: Fracture test
From: maghroudm@yahoo.fr
To: subramaniamdhanasekaran7@gmail.com; materials-welding@googlegroups.com

Dear sir.
Thanks a lot for your answer but also i need to know how can i interprete result after fracture test.

Best regard


Envoyé depuis un mobile Samsung


-------- Message d'origine --------
De : Dhanasekaran S
Date :22/06/2016 05:57 (GMT+01:00)
A : Materials & Welding
Cc : maghroudm@yahoo.fr
Objet : Re: Fracture test

Hi,


Please refer below image from ASME sec IX (QW462.4(c)) for fillet weld performance qualification.

As per drawing, cut the coupon and apply force.


  
  

Note: Also, you should carry out Macro test in order to qualify the welder (QW452.5).

  
  



Thank you.

Regards,
Dhanasekaran S,

Aker Solutions.

Mob: +91 75079 17709  I   +91 70401 02428 



On Wednesday, 22 June 2016 07:55:43 UTC+5:30, MAGHROUD Moussa wrote:

Dear expert.
I have to performe fracture test to qualify welders. The coupon is made by pipe 4"  to plate position 5F. My question is how to execute it?

Best regard


Envoyé depuis un mobile Samsung