Re: [MW:25020] Relation between diffusible hydrogen and welding current

Yes, diffusible hydrogen is more, more arc voltage is required to push the current due to bad conduct electricity by Hydrogen. Example 6010 is required more arc voltage when compared with 7018

On 28-Jun-2016 4:51 pm, <dilintas@gmail.com> wrote:
Research papers demonstrate the contrary

Sent from my BlackBerry 10 smartphone.
From: 'prem_nautiyal26' via Materials & Welding
Sent: Τρίτη, 28 Ιουνίου 2016 - 09:12
Subject: Re: [MW:25017] Relation between diffusible hydrogen and welding current


There is no relation between diffusible hydrogen content and Welding current.



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Pravin G <htcispravin@gmail.com>
Date: 27/06/2016 16:00 (GMT+05:30)
To: 'Agustin Jimenez' via Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25011] Relation between diffusible hydrogen and welding current

Dear expert,

What is the correlation between diffusible hydrogen and welding current.

How does Welding current affects diffusible hydrogen ? Based on any specific code or theory?

Kindly help to explain.

Pravin Poornachandran
Singapore
Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5DFF92D3-8F9F-4BA9-A964-E41BEB02E7CA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/v8q94dia7bqepf9lwwlby3f4.1467039768760%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160628061916.6713429.72666.3489%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOy9vhiNQauvGrm%2BX-KmPO77j%3DJZ7ShYP7zu2XWoX4fzg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...