Re: [MW:24731] RE: 24729] Welding of SB729 UNS NO8020

Pradip, what about 317 which has got more Mo than 320

On 22-Apr-2016 7:53 pm, "pgoswami" <pgoswami@quickclic.net> wrote:

Hi Rajesh,

If it involves welding or Alloy 20 to same , them ER320LR is the matching & ideal consumable. ERNiCrMo-3  will be over matching as well  as over priced. This filler could be used for dissimilar joints between alloy 20 and other alloys. Please seethe attachment for more details.

 
Thanks.

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
pgoswami@quickclic.net
pradip.goswami@gmail.com



-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA
Sent: Friday, April 22, 2016 12:58 AM
To: Materials & Welding
Subject: [MW:24729] Welding of SB729 UNS NO8020

Dear All
      Please  provide the guidlines of welding of SB 729 and B462 (alloy 20 ),i have selected the ER320LR and ERNiCrMo-3 for welding of Alloy 20, is it correct ?

plz reply
      

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9083c67a-d80a-41fb-bfc0-26c275834801%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAOLL9jWJnRlNiibrRouaze4BAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePjsCsxcP5gm0gr6Zy6_be0GU0B-NRJJgiSup2SYcB5ag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...