What is welding machine, if it is pulsed GMAW, u can use it for any thick, otherwise restrict to 13mm weld

On 17-Apr-2016 8:11 pm, "Jim Price" <JimPrice@polarcorp.com> wrote:
The limitations of MIG welding has a lot of Depends:
1. Depends on Base Material.
2. Depends on Welding Wire
3. Depends on Shielding Gas
4. Depends on Welding Mode and Transfer
5. Depends on Heat Inputs
6. Depends on Joint Design

Jim Price | Welding Engineer, CWI
Direct:  320.7463439 | Fax: 417-862-5564
jimprice@polarcorp.com







-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Shanmugananthan
Sent: Thursday, April 14, 2016 5:40 AM
To: Materials & Welding
Subject: [MW:24691] MIG welding process-reg

Dear Experts
Can we use MIG welding process for load carrying structural steel.... and also provide limitations of MIG welding process

Expecting your valuable suggestions

Regard
S.karthikeyan
Chennai

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d4a08674-c496-48d6-91df-9c49a35d8bd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2527edebf5c845f587d3e6d9a9e023f6%40POLARMAIL.PolarTank.local.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM_B36kANNQ42V574t1H2T1JZnfPwxzLsAbYkH7WyObqA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...