Sunday, April 17, 2016

Re: [MW:24705] Re: GTAW weld weaving

Its depends on the PQR.
Weaving tends to increase the heat input on the material.

On Apr 17, 2016 8:37 PM, "Vishwas Keskar Welding Manager Pune India" <vvkeskar123@gmail.com> wrote:
ASME SEC IX is lenient on weaving.WPS will guide this . Put the maximum weaving width  in WPS . With 2.4 dia , filler wire , a width of @12 mm is an acceptable width    

On Thursday, March 31, 2016 at 5:00:12 PM UTC+5:30, simon lawrence wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/467d2395-a259-4815-b8db-585cde441a74%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTWUJKQ%3Dws%3DBWb4kV9Hg9N17Ys8y2bXUNa05m_0ihL5Zw1gBw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...