Thursday, April 14, 2016

Re: [MW:24692] MIG welding process-reg

FCAW is better

Sent from my BlackBerry 10 smartphone.
  Original Message  
From: Karthikeyan Shanmugananthan
Sent: Πέμπτη, 14 Απριλίου 2016 - 13:57
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24691] MIG welding process-reg

Dear Experts
Can we use MIG welding process for load carrying structural steel.... and also provide limitations of MIG welding process

Expecting your valuable suggestions

Regard
S.karthikeyan
Chennai

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d4a08674-c496-48d6-91df-9c49a35d8bd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160414120441.6729807.9525.2634%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...