Thursday, April 14, 2016

Re: [MW:24689] Run-Out Length for SMAW Process

Hi
If you refer DIN EN ISO 15609-1 Spec. And qualifications of welding procedures clause 4.5.1 process 111; the run out length of electrode consumed or travel speed shall be mentioned in your procedure.

Regards

Prem Nautiyal
9769316004



Sent from Samsung Mobile


-------- Original message --------
From: 'prem_nautiyal26' via Materials & Welding
Date:13/04/2016 6:25 PM (GMT-05:00)
To: materials-welding
Subject: Re: [MW:24682] Run-Out Length for SMAW Process

Hi

Refer ASME Sec IX 2015 edition.
There is No such terminology called run out length mentioned ! 
Please ask your client for code reference. 

Regards

Prem Nautiyal
9769316004



Sent from Samsung Mobile


-------- Original message --------
From: Kurniatullah Sirajudin
Date:10/04/2016 12:30 AM (GMT-05:00)
To: Materials & Welding
Subject: [MW:24660] Run-Out Length for SMAW Process

Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb9ef69c-8c36-42e8-b090-7dd6d32d8af3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/x4wy765uvcnprjyvpuhdiica.1460589900305%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...