Thursday, April 14, 2016

Re: [MW:24682] Run-Out Length for SMAW Process

Hi

Refer ASME Sec IX 2015 edition.
There is No such terminology called run out length mentioned ! 
Please ask your client for code reference. 

Regards

Prem Nautiyal
9769316004



Sent from Samsung Mobile


-------- Original message --------
From: Kurniatullah Sirajudin
Date:10/04/2016 12:30 AM (GMT-05:00)
To: Materials & Welding
Subject: [MW:24660] Run-Out Length for SMAW Process

Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb9ef69c-8c36-42e8-b090-7dd6d32d8af3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...