Dear Experts,
Regarding fillet size minimum 70% of less thickness plate to be
considered.... And regarding plate qualification you have to just
conform as per drawing which plate material you are going top weld. If
it is mild steel then you can qualify IS 2062
Thanks,
Balamurugan,
L&T
On 4/13/16, 'prem_nautiyal26' via Materials & Welding
<materials-welding@googlegroups.com> wrote:
> Hi
> You have to refer approved construction drawing for the required fillet
> size.
> Else you may refer the construction code.
> If it is B 31. 3 then you may please use a 6mm size fillet.
>
> Regards
>
> Prem Nautiyal
>
>
>
> Sent from Samsung Mobile
>
> <div>-------- Original message --------</div><div>From: Vivek Pandey
> <vivek.pande06@gmail.com> </div><div>Date:12/04/2016 4:08 AM (GMT-05:00)
> </div><div>To: materials-welding@googlegroups.com </div><div>Subject: Re:
> [MW:24673] WQT fillet size </div><div>
> </div>Dear Tushar
> You can conduct fillet weld on pipe to plate as per section IX table
> QW-452.5 for guidence.
> Yes you can use IS2062 plate P-No. and Group No. that is mentioned table
> QW/QB-422 see section IX edition 2013
>
> On 12-Apr-2016 3:56 pm, "Tushar rao" <tushar.areva@gmail.com> wrote:
> Dear Experts,
>
> I want to cunduct fillet on pipe to plate. Pipe thk is 5.54 mm and plate thk
> is 10 mm.
>
> What is fillet size as per sec-9.
>
> And can i used IS 2062 plate in fillet test. Which was not mention in QW 422
> table.
>
> Please give feedback.
>
> Regards
>
> Tushar Rao
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/137fa05d-6826-4408-bf0c-94b4db82ad1c%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CANCwoY%3Dmhm68_HGBVFsXTJqWs4-UWmmjWRAL-F9Hgh35fpG3NA%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/2doumm4ljomu75toxue7wk93.1460554289063%40email.android.com.
> For more options, visit https://groups.google.com/d/optout.
>
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9C6DZ%3DSJtLhQpMcvNLgQRaxYOHes2a%3D4hEy%2B1BO061Htp9Hg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...