Wednesday, April 13, 2016

Re: [MW:24680] WQT fillet size

Hi 
You have to refer approved construction drawing for the required fillet size.
Else you may refer the construction code.
If it is B 31. 3 then you may please use a 6mm size fillet.

Regards

Prem Nautiyal



Sent from Samsung Mobile


-------- Original message --------
From: Vivek Pandey
Date:12/04/2016 4:08 AM (GMT-05:00)
To: materials-welding@googlegroups.com
Subject: Re: [MW:24673] WQT fillet size

Dear Tushar
You can conduct fillet weld on pipe to plate as per section IX table QW-452.5 for guidence.
Yes you can use IS2062 plate P-No. and Group No. that is mentioned table QW/QB-422 see section IX edition 2013

On 12-Apr-2016 3:56 pm, "Tushar rao" <tushar.areva@gmail.com> wrote:
Dear Experts,

I want to cunduct fillet on pipe to plate. Pipe thk is 5.54 mm and plate thk is 10 mm.

What is fillet size as per sec-9.

And can i used IS 2062 plate in fillet test. Which was not mention in QW 422 table.

Please give feedback.

Regards

Tushar Rao

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/137fa05d-6826-4408-bf0c-94b4db82ad1c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANCwoY%3Dmhm68_HGBVFsXTJqWs4-UWmmjWRAL-F9Hgh35fpG3NA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...