Re: [MW:24660] High YS to Low YS

It depends on Base Material P No and group No given in Sec IX and additional  requirements if any.

Best Regards,
Mohit Aggarwal.

On Apr 10, 2016 8:55 AM, "mubeenaws" <mubeenaws@gmail.com> wrote:

Good day all 
Please help me out by providing u r advise on below request. 

We have a qualified WPS with 75K YS material as per Sec-IX, can we use on material with 65K YS for welding? 

Please provide your feed back with reference clause. 

Thanks and Regards 
Munden


Sent from my Samsung device

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/rjpr5c1o0br8nc1ww9xs5w5r.1460209404507%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPPqk5%2BASMnp%2BP3h1c1d2R4XkWUzKatR7qbF6nZdXSZqEw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...