Sunday, April 17, 2016

[MW:24700] ASTM A672 Gr.C70 CL.32 Pipe Heat Treatment issues

Hi Experts,
As per ASTM A672 Gr.C70 Cl.32 heat treatment requires is normalized.
This normalizing requires either in which of the following condition? Please explain
1) After rolling and Welding of pipe. If requires what about the strength of weld which will reduce after normalizing and which welding consumables to be used to get higher strength.
Or
2) Plate Raw material requires to be Normalized.
 

Thanks & Regards
Krishna Mudhale
Mob.:+91-9860459776

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG8LsMYh58%2BN6B%2B_LXPa2Fs2OSXR4nJ-UDT3n5R9Cw6ZiV5tMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...