Re: [MW:24056] Re: UT in painted condition

This is the correct answer

Sent from my BlackBerry 10 smartphone.
From: dehsetengiz
Sent: Κυριακή, 3 Ιανουαρίου 2016 - 17:23
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24042] Re: UT in painted condition

UT of painted welds is possible, just you need to make sensitivity calibration on a block with same material and painted with same method.
But you Should take into account that,  there may be air gaps under paint which will cause missed sections



2 Ocak 2016 Cumartesi 17:21:08 UTC+2 tarihinde bala mani yazdı:
Hai,

whether UT can be done in painted condition??

Kindly share your opinions..  

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f390714f-d7a9-4fbe-95db-9b755e5bb20e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...