Better to put an insert. With such a large buttering you will accumulate a large amount of Heat input, unless you implement low heat input process and methodology.

Sent from my BlackBerry 10 smartphone.
From: Aby
Sent: Κυριακή, 3 Ιανουαρίου 2016 - 17:23
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:24041] Buttering gap

Hi all,

 

For a simple plate to plate joint of 40mm thickness can we do buttering of 100mm gap??

 

Regards,

Jose

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/011401d14612%24f7c19670%24e744c350%24%40com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...