Friday, January 1, 2016

[MW:24030] Re: Hydro test

what is code 31.4 or 31.3?
test mediam
test pressure
length of pipeline
line geomentry..


On Friday, January 1, 2016 at 4:05:02 AM UTC-8, nishanth km wrote:

Dear experts,

Is pressure drop(very small) acceptable in piping during hydro test beyond temperature variations. Please advice.

Regards

Nishanth

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bddd1279-e3d8-4574-a9e4-8c51ef9113da%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...