Re: [MW:23466] Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

You need to follows your code of construction (B31.3 in your case) in addition to ASME BPV IX. If piping is designed to B31.3, then you need to follow the requirements of B31.3

On 13 September 2015 at 01:23, Anban <gane2478@hotmail.sg> wrote:
Dear Sirs
Appreciate if you could provide clear and definitive response.

In my Yard Piping WPS/PQRs and Welders Qualification comply with ASME IX only.

ASME IX specifically developed as  Qualification Standard for Welding,Brazing, and Fusing Procedures;Welders; Brazers; and Welding,Brazing, and Fusing Operators
ASME B31.3- ASME Code for Process Piping.- (Design/Construction Code)


As For Welder/Operator/Brazer Qualification& Piping WPS/PQR Qualifications- what is mandatory code- ASME IX or Design/Construction Code ASME B31.3?


For example High Pressure Piping ASME B31.3 Chapter IX shall be complied for WPS/PQRs and Welder Qualifications.
Yes, PWHT requirements one need to comply with ASME B31.3-Table 331.1.1

Does that mean ASME IX requirements superseded by ASME B31.3 Chapter IX?
Where and when one shall comply with ASME B31.3 instead of ASME IX.?


Thanks


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DgMn%3Dh0-EgCMvKWYt%2BS0FYhSm4yYA%2BvL5E01xeEM8egw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...