Re: [MW:23447] WPS REVISION // Impact test temperature

As u r using consumable of superior grade,yes u can use but please ensure this WPS must not be used in case of non-impact requirement...because change of AWS class is a supplementary essential variable as per sec IX..

On 11 Sep 2015 9:20 am, "Raghuram Bathula" <raghurambathula@gmail.com> wrote:
No, you need to follow your code of construction and support with new PQR qualified at or below MDMT

On 11 September 2015 at 09:12, Mahesh Mirje <mahesh.mirje41@gmail.com> wrote:
Hi expert's,
I have PQR with electrode E7018, AND IMPACT tested at -30deg. Lets say Observed energy values 20J
Can I make wps with E7018-1, FOR IMPACT REQUIRMENT at -45 deg.required energy values 20j,
AS per ASME weld metal produced by 7018-1,  will provide 20j at -45 deg.
And HAZ ENERGY VALUES CAN BE CONTROLLED BY RESTRICTING HEAT INPUT.
Pls, clarify can I prepare wps for 7018-1 at -45 by restricting heat input as same used in 7018 PQR.

Regards
Mahesh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnJSKpehomULf6bXi%2Bv0%2BuKQesPQX2vT8KNC_YYacnnhw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAPe-FFCFSW2-K-xQ5U%2BFiF0aWhqS8SWbaF1x0SywcWKhubOhw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...