Tuesday, September 8, 2015

Re: [MW:23419] WPQ_ASME Section IX

Hi,

Performance qualification should be based on welding a qualified WPS or SWPS, So the welder could weld in the range of qualified thickness.

Refer to QW-301.2 for more details.

On Mon, Sep 7, 2015 at 1:25 PM, nut <baskaran.avc@gmail.com> wrote:
Dear experts,

Please advise on below query.

Ref Code: ASME Sec.IX

WPS Thickness range qualified  is 5- 22 mm

Can i conduct WPQ on 4mm or below thick plate or pipe using above WPS  if there is a necessity.

Or simply

Does anything restrict that the WPQ coupen thickness or diameter  should be within the qualified thickness range of referred  WPS?

Thank you.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ea15dfc-d965-4fe7-987a-3b96013dd5e1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts26%3DCsyT-8SsToEJH%3Du-vAjGpEsdYa4eRX1UDQ%3DL7i6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...