Re: [MW:23396] Vacuum pack welding electrodes

Dear Mr.Venkat,

Thank you very much for your reply. It is of great useful to me.





cordially,
Jay Poojary

On 5 September 2015 at 12:33, venkat chikkala <venkat_chikkala@yahoo.co.in> wrote:
Dear Jay,

Vacuum packed Low hydrogen electrodes, may be used without baking, if, packing is not damaged.

If electrodes are exposed to atmosphere same to be baked as per electrode  manufacture requirements or as specified by client specification.

You may refer  Table 3 in SFA-5.1 in ASME Sec II part C for baking temperatures &  para 5.3 in  AWS D 1.1 ( addition 2004) for storage of Low hydrogen electrodes.

Regards,
CH V Ramana
Bureau Veritas (I) Pvt Ltd.





On Saturday, 5 September 2015 11:44 AM, Jay Poojary <jayogini@gmail.com> wrote:


Dear Experts,
Can anybody from our experts,  share some information regarding vacuum pack low hydrogen electrode. Specially about the baking of this electrodes,  if left out.
Thanks & regards,
Jay Poojary,
QA/QC ENGINEER
OCLLC,
NIGERIA
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyQMm2T39_y9OaL-17NAe5bZhwiOVXKoh2YKpqLWEKV4RQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyQpTeT1v7M_5Tod8%2BC01GjWXTUd4ALXHmDS55C7KA2odA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...