Wednesday, September 2, 2015

Re: [MW:23384] PWHT thickness requirement as per ASME B 31.3 2014

HI Mohd,
 
As per ASME B31.3 Edition2014, there is the exception for PWHT for P1 Carbon steel materials.
 
A1.: Regardless of thickness, no PWHT for P1 Carbon steel Material if they meet the Limitation mentioned on the Table 331.1.3.
 
A2.: For carbon steel thickness > 25mm thickness, preheat of 95deg is an limitation for P1 material for avoiding PWHT.
 
Regards,
 
M. Sivachidambaram.
QHSE ENGINEER
GATES ENGINEERING & SERVICES.

On Tue, Sep 1, 2015 at 12:24 PM, S.Mohammed <mohd52100@gmail.com> wrote:
Dear all,

As old ASME B31.3-2012  we know it was above 19mm req pwht,

now i read ASME B31.3-2014,little confused me with pwht exemption and pwht requirements and control thickenss 331.1.3?

q1- what is thik req for pwht for P1 as per b31.3 2014 ?

q2 : for P1,mentioned more than 25mm thk and 95C preheat exemption from pwht so less than 25mm not require pwht ?


regards,
mohd.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33c22bce-8302-43cc-a853-e114ef80ace3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMVjbLvF4KUpvKWSjoyNGgWnP%2B76VRvgwVJB5Jj_bS5CNA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...