Sunday, September 6, 2015

[MW:23402] LTCS thickness range

What is basemtal thk.

Refer qw403.6 for base metal.range when impact applicable

t or 5/8t min..

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a94f9569-ac42-4de0-b895-cadc669d95bd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India