Hello,
Dear Colligious, can You give some adwises about the cladding (API, 6A) steel S32205 (1.4462) with Inconel 625.
What will be happen to grains? How will be changed ratio of Ferritic - Austenitic fractures? Will be appearing the danger of cracking?
What special methods (preheat, PWHT ...) I have to take?
Thank You. --
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFaoZORxLqz-Mw6%2Bp39oUszis%3Dd5ng3de-SEA3da7GCXZsrEYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Dear Colligious, can You give some adwises about the cladding (API, 6A) steel S32205 (1.4462) with Inconel 625.
What will be happen to grains? How will be changed ratio of Ferritic - Austenitic fractures? Will be appearing the danger of cracking?
What special methods (preheat, PWHT ...) I have to take?
Thank You. --
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFaoZORxLqz-Mw6%2Bp39oUszis%3Dd5ng3de-SEA3da7GCXZsrEYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments