RE: [MW:23115] Normal duplex and super duplex

Hello Pravin,
 
What's the  grade of DSS involved.What's the consumable used and what's the ferrite readings in consumable MTR? What's the thickness involved?
 
Meeting ferrite is only one part of DSS procedure qualification.
 
All those information would be worth looking at.
 
Thanks.
 
 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pravin G
Sent: Wednesday, April 15, 2015 10:04 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:23105] Normal duplex and super duplex

Dear Sir,

We used ferrite meter equipment.

Pravin Poornachandran


Sent from my iPhone

On 15 Apr 2015, at 15:15, meisam shokri arfaei <meisamshokri@gmail.com> wrote:

Which test did you implement for measuring the ferrite content?
Ferrite meter equipment or metallography?

On Wed, Apr 15, 2015 at 5:39 AM, Pravin G <htcispravin@gmail.com> wrote:
Dear expert,

I'm having to weld normal duplex plate for vessel, SMAW process with following requirements:

I.v -40degC
FN: 35-65
CPT 22deg C @24 hrs
Corrosion 4g/mm

I'm unable to achieve FN even after several test.

Can anyone guide me how to achieve FN ?

Pravin
Singapore

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C06614E3-D0AA-42F0-9BA6-9A63A4690B7C%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts043CrnjNht6Km%2BQy7MLfjSE-FhtVUJsz6-4%3Dbxq3oXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/53176D75-B09C-4089-B632-CB98FB845C12%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...