Dear Sir,

Do the radiography with selenium (Se-75) radioisotope. You will get the radiography film almost same as X-Ray.

This is a proven procedure for in-Situ radiography.  Engineers India Ltd(EIL), a leading Consultant and PMC firm, follows this procedure for radiography and we have done this successfully when worked for them.

Regards,

Hareesh K V

On Apr 23, 2015 9:25 PM, "Nitesh Patel" <nitesh.patel2@gmail.com> wrote:

Dear Dipak
As per my knowledge UT and PAUT is not possible due to austenite grain structure.

On Apr 23, 2015 5:40 PM, "deepak cb" <dcbvjs@gmail.com> wrote:
I would like to take NDT on Weld joints of 316 Pipe material Sch 10s. As per the site condition X-ray cant be used. And gamma source is also not available. Is there any other way. I mean Manual Ut or PAUT? Does the minimum thickness will be a problem if i go for Manual UT? please advise

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e1717216-36c2-4159-b1be-bd02fc1629fe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhgLaz%3Drx%3DK%2BDk0JuZRdpbJLAPyb8fJVUXUB5-5f4mdZNMPKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAU-a0NaR2fpWDKWrS-H_RxmaZkCpZq_Toqa7gGHDmcj%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...