Wednesday, April 15, 2015

Re: [MW:23100] Normal duplex and super duplex

You are getting low or high ferrite?

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Pravin G ---15/04/2015 06:29:23---Dear expert, I'm having to weld normal duplex plate for vessel, SMAW process with following requirem

From: Pravin G <htcispravin@gmail.com>
To: materials-welding@googlegroups.com
Date: 15/04/2015 06:29
Subject: [MW:23095] Normal duplex and super duplex
Sent by: materials-welding@googlegroups.com





Dear expert,

I'm having to weld normal duplex plate for vessel, SMAW process with following requirements:

I.v -40degC
FN: 35-65
CPT 22deg C @24 hrs
Corrosion 4g/mm

I'm unable to achieve FN even after several test.

Can anyone guide me how to achieve FN ?

Pravin
Singapore

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/C06614E3-D0AA-42F0-9BA6-9A63A4690B7C%40gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...