In your case, for 3mm, please see table 4-1 with SI units. you could find that:
- Any rounded indication which has dimension greater that 0.38mm is relevant. It means that defects smaller than this size should be discarded and won't affect your interpretation ( so 0.5mm rounded indication is relevant).
- All other defects shall interpret with those criteria which discussed in the Appendix 4.
Regards
On Fri, Apr 17, 2015 at 4:05 PM, Kanikumar Kumar <kanikumar1989@gmail.com> wrote:
Sir,--Thanks for your kind reply.I understood the max.size Rounded indication allowed for 3 to 6 mm.for example; 3 mm thk.According to fig 4-3, Can I consider below 0.79 mm defect as a non relevant indications?In this connection I am having 0.5 mm porosities 7 numbers Randomly... Can I accept?Kindly explain about relevant and non relevant indication..Thanks and regards,K.KANIKUMAR
On Wednesday, April 15, 2015 at 9:02:06 AM UTC+5:30, Kanikumar Kumar wrote:Dear Sirs,
I have some doubt regarding rounded indication (defects) in weld metal.
How much porosities (Numbers with size) are allowed in 3mm to 6mm material thk. According to ASME –VIII, Div-1 (Appendix 4)…
Because, In Appendix 4, FIG 4-3, lot of porosities are showed. So please Guide me.
Also suggest me how to read the standard with respect to Appendix-4.
I am waiting for your reply in this regards.
Thanks & Regards,
K.KANIKUMAR.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855b7c13-e85c-436d-a7db-5411263d420a%40googlegroups.com.
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer
Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtskR7-%2BBPP-4vQDEhNWyDWL-A0L7H9md%3D6BJa5LO5SmRw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments