Re: [MW:23174] How to qualify 1.5 mm thk to 60 mm thk in one wps

Dear All,

To my knowledge,  it's not possible.  Thank you.

Jay Poojary,
QC Engineer
Signate Engineers & Consultancy

On Apr 28, 2015 10:57 AM, "joydev dalai" <joykolkata07@gmail.com> wrote:
It is not possible 

On Tue, Apr 28, 2015 at 10:39 AM, pradip kumar Sil <pradipsil@gmail.com> wrote:
asme sec ix

On Mon, Apr 27, 2015 at 9:12 AM, S.Mohammed <mohd52100@gmail.com> wrote:
as per which code?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/31aa6d1b-9b75-459d-959a-c4d89cb70877%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kb4JmB9Y7NwbsaehrNjhHeTyS551%2BUDU_hUW1785kDXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--



Best Regards,

Joydev Dalai
Sr. Engineer - QA/QC
Kalpataru Power Transmission Ltd
KJPL Project,(Spread-1)
Mob :- +91-7728885768

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFQz-VL80TEWrH%3D5HscjuPUd3ELOwa08Rqbf09%3Dwu_9JrjW2hg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyRcmuP1a1L6A68Zqk3L%2B2qPycA2MF%2BbUvYd6y%3DbxTttXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...