Please refer the interpretation below.


Status:  Currently Valid
Other Links:
________________________________________________________________________________   
Interpretation:    IX-83-169
Subject: Section IX, QW-404.9
Date Issued: May 14, 1985
File: BC85-089

Question: For submerged-arc welding, can a fabricator use a different brand of flux than that specified in a wire-flux classification for which he is qualified, without performing a new PQR?

Reply: No.


Best Regards,
Gurunathan.R

On Wed, Apr 15, 2015 at 5:22 PM, Mhaskar Aly <mhaskar.aly@gmail.com> wrote:

Dear All,

We have PQR of following details:

 

Process SAW with Filler Wire EM12K (ESAB) with Flux F7A8 (ESAB OK 10.62 Flux)

 

Question:

1.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (ESAB OK 10.62 Flux)

2.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (Bohler Flux)

 

Kindly advise as per ASME Sec IX…with reference.

 

Thanks in advance

 

Thanks & regards

 

Ali Mhaskar,

QA/QC Manager

Velath Engineering International FZC; Hamriyah FreeZone Sharjah, UAE; * P.O Box 6268 – Sharjah UAE.
(Phone: 00971-6-526 9269, 526 9185, 526 9119 Ext-212 ÈMobile no.: 00971-55 265 3598 ÊFax no. 00971-6-526 9393  üwww.velath.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4htWh-B5O0xAn_yPAbYpWWRcX6NWmDT5tmmziG3jgPAxQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACt3NQMvdpRSdPy5%3DYtKhQPuHW58N8oxHWbeaP6xnSqws%3DC3Sg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...