All NDT methods should be done based on a written procedure. 

This written procedure should contain any criteria for doing such method and further action after NDT execution. Generally UT is not a common method for thicknesses thinner than 6mm (some standards mentioned 8mm). Please note that UT is not common but may use in few cases.

The thickness is one of the issues you should concern about and the other will be the nature of your material (austenitic structure). Selection of the probe size and frequency will be very important.

Also the type of discontinuities and their position and orientation will be the case.

My answer is a general one and in your case, consult with a NDT expert to write a procedure for your case.

Regards

On Thu, Apr 23, 2015 at 4:26 PM, deepak cb <dcbvjs@gmail.com> wrote:
I would like to take NDT on Weld joints of 316 Pipe material Sch 10s. As per the site condition X-ray cant be used. And gamma source is also not available. Is there any other way. I mean Manual Ut or PAUT? Does the minimum thickness will be a problem if i go for Manual UT? please advise

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e1717216-36c2-4159-b1be-bd02fc1629fe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtvfktoNDKzWP0u%3DNkKLMFe8kJTGW9WUZCDaf1eS2u9QqQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...