Re: [MW:23129] Clarification of SA572 Cu content.

it's the PO

Best Regards

Ramin Kondori

Sr. QA/QC engineer

Yadavaran Oilfield Project

SIPC (SINOPEC)


On Sat, Apr 18, 2015 at 10:57 AM, Biplab Pal <biplab.mech@googlemail.com> wrote:
Dear Experts,

I have a doubt of the interpretation of SA572
I chemical analysis it states "A Copper when specified shall have a minimum content of 0.20% by heat analysis (0.18% by product analysis)."

I want to interpret the meaning of specified. Is it PO or MTC.

My case is, contractor has purchased the material of structural steel. Their PO dose not mentioned that certificate need to me mentioned about Cu content, but in Lab test certificate the % of Cu is mentioned and it comes below the minimum requirement. The material shall be accepted or rejected.

Can you please clarify the matter.
I am expecting your valuable input and reply.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0on-_jtshy7rkaGpQdiBD55t8q7FUtQZuu%3DDpcZy%2Bdmg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUhomTL7Xr22KXsM6n4O4FFD-qDiAoD5Y1vO%2B_aoLZCeHg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...