Wednesday, April 29, 2015

Re: [MW:23187] PQT for A333 Gr.6 pipe

Hi,

What you have mentioned is one of the option. or you can directly weld pipe to flange and carryout the procedure qualification for which you may have to procure additional flanges.

Regards,

L. Prabhu kumar
Ph. no. 9003010978


From: "'ramen samanta' via Materials & Welding" <materials-welding@googlegroups.com>
Sent: Wed, 29 Apr 2015 09:32:08
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: [MW:23181] PQT for A333 Gr.6 pipe
Dear Experts,

In our project, we have to establish a  WPS /PQR for A333 Gr 6 Pipe (P-1,Group-1) and Flanges A350 LF-2 (P-1,Group-2).   Process - GTAW+SMAW (with ER 70S-2 and E7018-1).

How to conduct/establish one combined PQT with P-1,Group-1 to P-1,Group-2 ?? 

Can we make two PQT separately of below options :-

One Pipe to Pipe in 6G position and other any Plate to Plate in 4G/3G position of which Tensile Strength 70 ksi) - Is it acceptable  as per ASME Sec-IX?


Please clarify.
 
Thanks in advance,

R.K.Samanta

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/557282115.432383.1430235096703.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1430280128.S.18193.8497.f5-224-163.1430300104.12976%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...