Re: [MW:23103] Stud Welding

Please read QW-192 for tests in WPS and/or welder qualification.
Also read QW-261 for essential variables.

Regards

On Wed, Apr 15, 2015 at 2:31 PM, pankaj phuse <pankaj.phuse@gmail.com> wrote:
Stud Material :SA 193 GR.B7
Plate Material:IS 2062 GR.B

Dear experts,
How to qualify WPS For the stud to plate welding for the above mentioned details,as per ASME Sec IX.

Regards,
Pankaj

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a05deb5a-80a0-4859-a4f2-7180c7bd203b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtsBgrZozKmpbaw%3DdwAk1BkWSsCferCGtyjbW5YRJbnC9Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...