Sorry for the error..what I intended to suggest  was the dissimilar combination of PIG1 and P1G2 can be achieved if both pipes are used..

On 30-Apr-2015 9:48 AM, "MUNHOZ Sergio TECHINT" <tbrsmu@techint.com.br> wrote:

Dear Sirs

 

·        A333 Gr 6 is P1 G1 and not P1 G2

 

·        Question: Under B31.3; Impact test required; can I combine one single Pipe to Pipe P1 G1 PQR with  one single Pipe to Pipe P1 G2 PQR and issue one Pipe P1 G1 X Pipe P1 G2 WPS ?

 

Best regards

 

 

Sergio Munhos

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PUB:K.M Hrishikesan
Sent: quarta-feira, 29 de abril de 2015 07:36
To: materials-welding
Subject: Re: [MW:23188] PQT for A333 Gr.6 pipe

 

If you want to use pipes, you can run the PQR using A333 Gr 6 and API 5L X65 pipes , both are P1G2 materials. Hope there is impact test requirements.

Dear Experts,

 

In our project, we have to establish a  WPS /PQR for A333 Gr 6 Pipe (P-1,Group-1) and Flanges A350 LF-2 (P-1,Group-2).   Process - GTAW+SMAW (with ER 70S-2 and E7018-1).

 

How to conduct/establish one combined PQT with P-1,Group-1 to P-1,Group-2 ?? 

 

Can we make two PQT separately of below options :-

 

One Pipe to Pipe in 6G position and other any Plate to Plate in 4G/3G position of which Tensile Strength 70 ksi) - Is it acceptable  as per ASME Sec-IX?

 

 

Please clarify.

 

Thanks in advance,

 

R.K.Samanta

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/557282115.432383.1430235096703.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFHBd_9E_ozZsURVyuZvfheDVZHfyo3WuKx%2BA-%2B_hh_4dm7G8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/A7B6894BA272C24C889548CCE8FDAE9B36168F75%40TEIBRWEXMBX100.teic.techint.net.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFHBd__fjVQwrtfCNMCif9TXq9j-jSpyt6%2BMsg%3DogQ9UfHS5qw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...