Wednesday, April 22, 2015

Re: [MW:23141] J groove bevel end requirement

No it is not. The form of bevel in compromise between accessibility and volume of deposited weld metal

Sent from my BlackBerry 10 smartphone.
From: Prabhakar Raj
Sent: Τετάρτη, 22 Απριλίου 2015 - 06:55
To: materials-welding@googlegroups com
Reply To: materials-welding@googlegroups.com
Subject: [MW:23137] J groove bevel end requirement

Can anyone give me code reference for J groove bevel end  requirement above 22mm wall thickness.  Is it mandatory to go for J groove.?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w9oYr_5Wb2e8MxKXSn_oWGa2YDv%2BQkOheTDE-D_ZoYRgA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...