If you want to use pipes, you can run the PQR using A333 Gr 6 and API 5L X65 pipes , both are P1G2 materials. Hope there is impact test requirements.

Dear Experts,

In our project, we have to establish a  WPS /PQR for A333 Gr 6 Pipe (P-1,Group-1) and Flanges A350 LF-2 (P-1,Group-2).   Process - GTAW+SMAW (with ER 70S-2 and E7018-1).

How to conduct/establish one combined PQT with P-1,Group-1 to P-1,Group-2 ?? 

Can we make two PQT separately of below options :-

One Pipe to Pipe in 6G position and other any Plate to Plate in 4G/3G position of which Tensile Strength 70 ksi) - Is it acceptable  as per ASME Sec-IX?


Please clarify.
 
Thanks in advance,

R.K.Samanta

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/557282115.432383.1430235096703.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFHBd_9E_ozZsURVyuZvfheDVZHfyo3WuKx%2BA-%2B_hh_4dm7G8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...