Monday, April 27, 2015

[MW:23167] Require electrode / filler wire details for CR weld overlay on CS with SS 316L

Dear Experts,

I would like to ask what type of electrode or filler wire need to be use for Corrosion resistance weld overlay on CS (P1 Gr 1 material) with SS 316L for SMAW, GTAW and GMAW processes.
And also which type of welding process will be suitable for Flange face weld overlay with SS 316L.
Your kind support in this regards is anticipated.


Thanks and Regards,
Mohammed Chand.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACdbzv_SzRbF5wAaXYagTn0q0OXerC6AHyqzCjUifKRqgvdetg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...