Re: [MW:23173] How to qualify 1.5 mm thk to 60 mm thk in one wps

butt weld of fillet weld?

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


pradip kumar Sil ---27/04/2015 16:36:26---Dear All, I want to make one wps 1.5 mm thk to 60 mm SMAW process carbon steel

From: pradip kumar Sil <pradipsil@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Date: 27/04/2015 16:36
Subject: [MW:23168] How to qualify 1.5 mm thk to 60 mm thk in one wps
Sent by: materials-welding@googlegroups.com





Dear All,
I want to make one wps 1.5 mm thk to 60 mm SMAW process carbon steel material. so can anyboby inform me how can I make it
Regards
Pradip

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8np8jG4eb2KUs1fkTsmhC030FEQZ2J6QB%2B3OGhZexP1aQ%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...