Re: [MW:23182] Require electrode / filler wire details for CR weld overlay on CS with SS 316L

Better u can apply ER 309LMo and Second Layer ER 316L.

Regards
Suryakant

On Mon, Apr 27, 2015 at 7:13 PM, S.Mohammed <mohd52100@gmail.com> wrote:
fisrt layer  ER 309 and second layer ER 316L.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5fe586ae-70bf-437f-bb56-a816b42442f8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPajZgaF79Z9XOZc-MFDGFCBLXjwnmrRS2CJLUCjHS%2BW7Om1Og%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...