Sir,
Thanks for your kind reply.
I understood the max.size Rounded indication allowed for 3 to 6 mm.

for example; 3 mm thk.
According to fig 4-3,  Can I consider below 0.79 mm defect as a non relevant indications?

In this connection I am having 0.5 mm porosities 7 numbers Randomly... Can I accept?

Kindly explain about relevant and non relevant indication.. 

Thanks and regards,
K.KANIKUMAR






 


On Wednesday, April 15, 2015 at 9:02:06 AM UTC+5:30, Kanikumar Kumar wrote:

Dear Sirs,

I have some doubt regarding rounded indication (defects) in weld metal.

How much porosities (Numbers with size) are allowed in 3mm to 6mm material thk. According to ASME –VIII, Div-1 (Appendix 4)…

Because, In Appendix 4, FIG 4-3, lot of porosities are showed. So please Guide me.

 

Also suggest me how to read the standard with respect to Appendix-4.

 

I am waiting for your reply in this regards.

 

Thanks & Regards,

K.KANIKUMAR.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855b7c13-e85c-436d-a7db-5411263d420a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...