Re: [MW:22372] Corrosion on SS Pipe

wrong material selection as 304 not recommended for maritime environment
as maritime environment cause stress corrosion cracking (ssc) on austunitic stainless steel, replace  material to duplex or super duplex or super austunitic.
the best is super austunitic ( 904L) then super duplex then duplex.

On Tue, Nov 25, 2014 at 7:43 AM, Sergio Antonio Muñoz Pinzón <seanmup@gmail.com> wrote:
Prince could you please describe better the corrosion, is it pitting or general corrosion? Do you have pictures?

Sergio Muñoz
IWE-IIW
http://Weld-ING.blogspot.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...