[MW:22345] Re: MATERIAL GROUPING IN API RP2A

Ali,

0,45% CEq is not so high, it's an intermediate value, cracking could appear in steels with different CEq (low or high) if non adequate welding procedure is used.
Material selection for each element depends on the particular design considerations (loads, temperature, corrosion consideration, etc), if the legs are going to be exposed to low temperatures design must take this in consideration, choosing an improved toughness material.

Sergio

El lunes, 24 de noviembre de 2014 03:19:08 UTC-5, Ali Asghari escribió:
Dear Sergio
Thank you for responding.
1-I think Carbon equivalent ranges of up to 0.45% and higher is permitted due to limitation of strength. because even welding use low hydrogen in higher this range the possibility of cracking is high.
 2-Do you have any design reference about category of redundancy of structural member or critically of them. because in previous projects acc. to AGIP or TOTAL spec. these items are primary members and in 8.3.1,8.3.2 use of class A,B or improved toughness property is recommended for legs. 
3- Do you have any example about  application of 11.1.3 b(fabrication sequence)?
Regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...